<ruby id="r7nf9"></ruby>
        <address id="r7nf9"><output id="r7nf9"><span id="r7nf9"></span></output></address><address id="r7nf9"><mark id="r7nf9"><dl id="r7nf9"></dl></mark></address>

          <ruby id="r7nf9"></ruby>
            <address id="r7nf9"><strike id="r7nf9"><p id="r7nf9"></p></strike></address>
                <dfn id="r7nf9"></dfn>

                            <dfn id="r7nf9"></dfn>

                                  <address id="r7nf9"><listing id="r7nf9"><menuitem id="r7nf9"></menuitem></listing></address>
                                  <address id="r7nf9"><mark id="r7nf9"><menuitem id="r7nf9"></menuitem></mark></address>

                                      <ins id="r7nf9"></ins>
                                      <address id="r7nf9"></address>

                                      <em id="r7nf9"></em>
                                        <ins id="r7nf9"></ins>

                                      膩子粉墻面掉粉的原因及處理方法

                                      點擊次數:   更新時間:20/03/31 15:56:03     來源:www.desenchantee.com 分    享:

                                        室內裝修的過程中通常都會在墻面打一層膩子粉,但由于各種原因偶爾會出現脫粉的情況,在這里威海膩子粉廠家給大伙講講其中的原因及解決辦法:
                                        一、原因
                                        1、施工原因:因為油漆師傅在最終一道收光施工時屢次用刮刀干刮墻面而引起的外表纖細的起皮現象,等干燥后就會構成脫粉癥狀。
                                        2、人為原因:因為最終一道施工膩子未干時,遇到外來粉塵附著到墻面上(切割作業,大風,清理地板等)導致的墻面假象脫粉。
                                        3、出產原因:因為出產人員大意將原料配方比例放錯,或因機臺設備卸漏,導致的配方不穩定而引起的脫粉。
                                        二、處理辦法
                                        1、施工師傅在做最終一道不上漆收光施工時應留意膩子的外表濕度,太干時會引起起皮脫粉,在收光時將刀痕修平即可,不宜屢次干刮。
                                        2、如出現粉塵附著在墻面上形成的假象脫粉的應待裝飾結束后用雞毛彈清除粉塵,或用清水與干凈的布條擦洗干凈即可。
                                        3、如出現快干脫粉的,應等公司技術人員到現場鑒定是否是因為產品配方引起的原因。

                                        以上就是威海膩子粉廠家帶給大伙的有關知識了,更多精彩內容歡迎關注我們的定期更新,會對您有所幫助的。